Send Message

Hastelloy C276 Welding Wire Hastelloy Alloy Wire With Excellent Stress Corrosion Cracking Performance

Negotiation
MOQ
Negotiation
Price
Hastelloy C276 Welding Wire Hastelloy Alloy Wire With Excellent Stress Corrosion Cracking Performance
Features Gallery Product Description Request A Quote
Features
Specifications
Standard: AISI, ASTM, BS, DIN, GB, JIS, Other,JIS,AISI,ASTM,GB,DIN,EN
Grade: Hastelloy C276
Place Of Origin: Jiangsu, China (Mainland)
Type: Wire
Special Use: Heat Exchanger
Delivery: 25-30 Days Subject To The Clients' Requirements And Quantity
Price Term: Ex-Work,FOB,CNF,CFR,CIF,FCA,DDP,DDU
Application: Industry
Highlight:

hastelloy c276 forging

,

hastelloy c22 pipe

Basic Infomation
Place of Origin: Jiangsu, China (Mainland)
Brand Name: BLM-HA-1
Payment & Shipping Terms
Packaging Details: packed and labeled according to the regulations and customer's requests.Great care is taken to avoid any damage which might otherwise be caused during storage or transportation.
Delivery Time: 25-30 days subject to the clients' requirement and quantity
Payment Terms: Western Union, L/C, T/T
Supply Ability: 300 Ton/Tons per Month
Product Description

                       

Good price nickel alloy hastelloy c276 wire price

 

Chemical composition:

 

  C S Mn P S Ni Cr Mo Fe Co W V
Min             14.5 15.0 4.0   3.0  
Max 0.01 0.08 1.0 0.04 0.03 Margin 16.5 17.0 7.0 2.5 4.5 0.35

 

Hastelloy C-276 Physical properties:

Density 8.9 g/cm³
Melting point 1325-1370 ℃

 

Hastelloy C-276 alloy minimum mechanical properties in the room temperature

Alloy state Tensile strength Rm N/mm² Yield strength R P0. 2 N/mm² Elongation A 5 %
C /C276 690 283 40

 

 

 

Characteristic as below

1. Excellent corrosion resistance to most of corrosion media in oxidation and reduction environments.

2. Excellent resist pitting, crevice corrosion and stress corrosion cracking performance.

 

Hastelloy C-276 Metallurgical structure C276 is face-centered cubic lattice structure. Hastelloy C-276 Corrosion resistance C276 alloy suit for many kinds of chemical process industry which contain the oxidizing medium and reductant.

High molybdenum and chromium content make it can resist the chloride corrosion, and tungsten make it corrosion resistance better.

C276 is one of a few material that can resist the corrosion of most chlorine, hypochlorite and chlorine dioxide, this alloy have prominent corrosion resistance to high concentration chlorate( iron chloride and copper chloride).

 

 

Hastelloy C276 Welding Wire Hastelloy Alloy Wire With Excellent Stress Corrosion Cracking Performance 0

 

Recommended Products
Get in touch with us
Contact Person : Kara Liu
Tel : 0086-13914912658
Fax : 86-512-89598069
Characters Remaining(20/3000)