Nitronic 60 Steel Wire , Corrosion-resistant
1.Description:
stainless steel known for it’s excellent galling resistance. It has oxidation resistance similar to alloy 309 stainless and maintains some moderate strength up to 1800°F. This alloy has about twice the yield strength of 304 with better corrosion resistance, falling between alloy 304 and alloy 316L.
2.Chemistry Typical
Carbon: 0.10 max
Manganese: 7.00-9.00
Silicon: 3.5-4.5
Chromium: 16.00-18.00
Nickel: 8.00-9.00
Nitrogen: 0.08-0.18
3.Physical Properties
Density: 0.275 lb/in³, 7.622 g/cm³
4.Mechanical Properties at Room Temperature
Properties: Annealed Typical
Ultimate Tensile Strength: 105 KSI nom (724 MPa nom)
Yield Strength: 55 KSI nom (375 MPa nom )
Elongation: 50% min
5.Standard Wire Finishes
Extra Clean: (XC) Extra clean is also referred to as “bright annealed” or “bright annealed and cold rolled”
Grease (round wire only): Drawn in a heavy grease produces an “Ultra bright” finish for decorative applications
Soap (round wire only): Soap is used as a lubricant in the drawing process and is not removed. It acts as a lubricant during customer part forming operation. A soap finish is available in tempered products.
Plated: Many plating options are available.
∗Special finishes are available: Contact Ulbrich Wire Sales with special finish and plating requests.